    Abstract:

    Si3N4 powders have been pre-treated by shock activating and hot-pressed into Si3N4 ceramics. Three kinds of shock pressure, and three different sintering temperatures are used in the experiments, SEM, TEM and X-ray Diffraction have been used to analysis the structure of the Si3N4 powders and ceramics. The properties of Si3N4 ceramic have been tested. The results show that shock activation give positive action to the densification of Si3N4 powder and the increase of properties of the Si3N4 ceramics; the ceramic parts shocked under 40 GPa and sintered under 1800℃ have the best properties. The bend strength reaches 1107.2 MPa, at the same time, the fracture toughness reaches 12. 20MPa.m1/2.

    Reference
    Related
    Cited by
Get Citation
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:September 01,1999
  • Revised:
  • Adopted:
  • Online: November 18,2013
  • Published:
Article QR Code