Low dielectric constant material which substitutes for conventional SiO2 thin film as intermetal dielectric (IMD) is imperative for the reduction of interconnect resistance/capacitance(RC), cross talk and power consumption. SiO2 aerogel film with unique properties such as ultra-low dielectric constant, low density and high thermal stability is one of the most possible candidates as IMD. SiO2 aerogel films on a silicon wafer have been synthesized via a process of sol-gel, spin coating and supercritical drying. SiO2 sol is prepared using a two-step procedure with acid/base as catalyst to investigate the effect of different amount of isopropanol(IPA) and NH4OH on sol viscosity which is important for spin coating and the microstructure of SiO2 aerogel film. The optimized viscosity of SiO2 sol is in the range of 9~15 mPa·s. It is found that the time of viscosity in 9~15 mPa·s becomes longer as IPA increases or NH4OH decreases.
参考文献
相似文献
引证文献
引用本文
王娟,张长瑞,冯坚.溶胶—凝胶法制备SiO2气凝胶薄膜溶胶粘度的研究[J].国防科技大学学报,2003,25(6):30-34. WANG Juan, ZHANG Changrui, FENG Jian. Viscosity of SiO2 Sol for Preparing SiO2 Aerogel Filmby Sol-gel Method[J]. Journal of National University of Defense Technology,2003,25(6):30-34.