Fabrication of Cf/SiC Composites by Pyrolysis PrecursorPCS/DVB at High Heating Rates
DOI:
CSTR:
Author:
Affiliation:
Clc Number:
Fund Project:
Article
|
Figures
|
Metrics
|
Reference
|
Related
|
Cited by
|
Materials
|
Comments
Abstract:
Three-dimensional braided carbon fiber (3D-B CF) reinforced SiC composites were fabricated via infiltration and pyrolysis of polycarbosilane(PCS)/divinylbenzene (DVB). The results show that increasing pyrolysis heating rates can reduce cycle time of manufacturing. At the same time, it can increase the density of Cf/SiC materials and improve the interface between carbon fiber and SiC matrix. The flexural strength of Cf/SiC materials reachs 556.7MPa.
Reference
Related
Cited by
Get Citation
JIAN Ke, CHEN Zhaohui, MA Qingsong, Zheng Wenwei. Fabrication of Cf/SiC Composites by Pyrolysis PrecursorPCS/DVB at High Heating Rates[J]. Journal of National University of Defense Technology,2003,25(2):30-33.