    The alcogel prepared by sol-gel process of polydiethoxysiloxane (PDEOS) according to the mass ratio of C2H5OH∶ PDEOS∶HF∶H2O=20∶10∶3∶0.5, was modified by methyltriethoxysilane(MTES) and washed with alcohol and n-hexane. The obtained gel was then dried under ambient pressure to prepare hydrophobic SiO2 aerogel. It is shown that hydrophobic SiO2 aerogels can be obtained when the mass ratio of MTES/ PDEOS is higher than 1.2. The contact angle between hydrophobic SiO2 aerogels and water is larger than 110°, the densities and specific surface areas of hydrophobic SiO2 aerogels are in the range of 125~160kg/m3 and 560~900m2/g respectively.

    Reference
    Related
    Cited by
Get Citation

CHEN Yimin, XIE Kai, HONG Xiaobin, XIAO Jiayu. Preparation of Hydrophobic SiO2 Aerogels at Ambient Pressure[J]. Journal of National University of Defense Technology,2005,27(2):11-14.

Copy
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:October 09,2004
  • Revised:
  • Adopted:
  • Online: March 25,2013
  • Published:
Article QR Code