    The conversion process of the polycarbosilane (PCS) into silicon carbide (SiC) was investigated by TG-DTA, infra-red spectrum analysis (IR) and X-ray diffraction (XRD) etc, which indicated the quasi ceramic characteristics of pyrolyzates treated at 600℃. The carbon fiber reinforced silicon carbide (Cf/SiC) composites were hereby prepared at 600℃ through precursor infiltration and pyrolysis (PIP), and polycarbosilane (PCS) acted as precursor, carbon fiber as enhanced fiber. The results show that bending strength of 3D-Cf/SiC composites are 193.69MPa, room tensile strength 197.69MPa, high temperature(600℃) tensile strength 167.33MPa. Noticeably, the density of 3D-Cf/SiC composites is just only 1.27g/cm3. Furthermore, the fracture surface and microstructure were analyzed and discussed too.

    Reference
    Related
    Cited by
Get Citation

ZHOU Changcheng, ZHANG Changrui, HU Haifeng, ZHANG Yudi, WANG Zhiyi. Preparation of Quasi Ceramic Cf/SiC Composites[J]. Journal of National University of Defense Technology,2008,30(2):41-45.

Copy
Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:October 25,2007
  • Revised:
  • Adopted:
  • Online: December 07,2012
  • Published:
Article QR Code